In Situ Movie of SWNT SuperGrowth.

In situ movie of 2-mm-thick SWNTs growing in 7 min.
Combinatorial catalyst library of Fe/Al2O3 was used,
in which Fe thickness varied from 0.2 nm (left) to 3 nm (right).
Note that SWNTs show bright red color at the elevated growth temperature.